    The Requirements of Pressure Vessel in Nonferrous Metals especially in Titanium and Nickel

    Requiements of Ti/Ni Pressure Vessel


    Compression of titanium pressure vessel manufacturing components, shall meet the following requirements
    1. Design temperature: pure titanium should not higher than 230 ℃, titanium alloy should not higher than 300 ℃, titanium/Steel clad plate should not be higher than 350 ℃.
    2. Pressure vessel shell of titanium material should be used in the annealed state.
    3. Titanium pressure vessel head forming hot forming or hot after cold forming to straighten. For forming of titanium steel clad plate head, ultrasonic testing should be done.
    4. Titanium pressure vessel is generally not required heat treatment, the use of titanium in stress corrosion environment in the container or use titanium plate made of container, or hot working after welding shall be carried out after eliminating stress annealing. Titanium steel clad plate after explosion compound, eliminate stress annealing treatment should be done.
    5. Titanium pressure vessel weld penetration test should be:
    (1) Nozzle, flange, reinforcing ring and shell or head connection fillet weld;
    (2) Heat exchanger tube and plate connected to the pipe weld;
    (3) Titanium steel clad plate cladding weld and fillet cover plate with composite panels lap weld cladding.
    Nickel material manufacture pressure vessel pressure parts, shall meet the following requirements:
    1. The design temperature, in the annealing state of pure nickel material should not be higher than 650 ℃, nickel copper alloy should not be higher than 480 ℃, Ni - Cr - iron alloy should not be higher than 650 ℃, nickel - iron - chromium alloy should not be higher than 900 ℃.
    2. Mainly used in the manufacture of pressure vessel pressure parts of nickel material should be used in annealing state, heat exchanger with linear nickel pipe should be used in eliminating stress annealing conditions.
    3. The nickel material head of pressure vessel using hot forming should be strictly control heating temperature. For forming nickel steel composite panels, ultrasonic testing should be done.
    4. Hot forming nickel material of heating temperature and heating and heating furnace atmosphere shall be strictly controlled, prevent pollution of sulfur brittleness. Recommend hot working temperature range is:
    (1) Pure nickel (N6-2.5-1, 5) is 280 ~ 350 ℃;
    (2) Monel (NCU28-2.5-1.5) for 350 ~ 500 ℃;
    (3) Inconel (NS312) is 470 ~ 550 ℃;
    (4) Hastelloy (NS334) is 930 ~ 1200 ℃.
    Nickel material of the pressure vessel magnetic particle or liquid penetrant welds shall be of the following:
    (1) Nozzle, flange, reinforcing ring and shell or head connection fillet weld;
    (2) Heat exchanger tube plate connected to the pipe weld;
    (3) Nickel steel composite board of cladding welding joint.


    国产精品久久久亚洲456 | 蜜桃麻豆www久久国产精品| 国产精品无码素人福利不卡| 精品视频在线观看你懂的一区| 影音先锋最新资源网| 精品国产一区二区三区久久久狼| 亚洲午夜精品久久久久久人妖| 久久99精品免费一区二区| 亚洲精品中文字幕乱码三区| 久久精品国产91久久麻豆自制| 精品第一国产综合精品蜜芽| 亚洲精品在线视频| 国产女人精品视频国产灰线 | 亚洲国产精品日韩| 国产精品一区二区久久国产| 一本久久a久久精品综合夜夜 | 美女黄页免费视频大全在线| 99久久99久久久精品齐齐| 国内精品久久久久久不卡影院| 野狼第一精品社区| 91国内揄拍国内精品情侣对白| 在线观看国产永久免费| 国内精品伊人久久久久| 日韩午夜高清福利片在线观看欧美亚洲精品suv | 日韩欧美亚洲国产精品字幕久久久 | 久久精品麻豆日日躁夜夜躁| 97精品人妻一区二区三区香蕉 | 成人精品一区二区三区中文字幕| 国产精品无码久久四虎| 亚洲午夜国产精品无码| 99国内精品久久久久久久| 美女扒开尿口给男人桶动态图| 欧美+亚洲+精品+三区| 台湾佬美性中文网| 国内精品久久久久久野外| 最近中文字幕免费4| 久久精品九九亚洲精品天堂| 亚洲国产精品成熟老女人| 亚洲国产成人精品不卡青青草原| 日本精品一区二区三区在线播放| 四虎国产精品永久地址99|